Introduction
Adding silver to leaded solder paste can significantly improve its fluidity, enhance soldering reliability, and greatly optimize the low-impedance performance of solder joints after welding. Today, KEWEI factory introduces a moderately priced lead solder paste with good soldering performance: metal composition – Sn62.8/Pb36.8/Ag0.4.
Developed for the evolving SMT rapid chip soldering process, this no-clean solder paste exhibits minimal residue after welding, with the residues offering high insulation impedance performance. It fully meets the no-clean requirements of SMT chip mounting processes in electronics factories.
Product Name | Solder Paste |
---|---|
Model No. | KWSP-628 |
Melting Point | 179-183℃ |
Particle Size | 20-38 μm |
Flux Type | ROL0 |
Composition | Sn62.8Pb36.8Ag0.4 |
Flux Content | 10±0.5 |
Viscosity | 170±30 |
Shelf Life | 6-12 Months (0-10℃) |